Thursday, June 18, 2015

[MW:23087] Re: Whether we can weld SA 335 P11 and SA 335 P91

it is
OD 60.3mm and Thickness= 11.07mm
pressure = 6 bars
temp= 585 c
it is an butt weld

it is not an condensing system it is an MAV system ( Lubricant supply system )



On Wednesday, June 17, 2015 at 7:29:47 PM UTC+5:30, arunkumar periasamy wrote:

In my condensing system my header line is having 2 materials

The line above sprayer which was connecting with condenser is SA 335 P11

And after sprayer till loop is SA 335 P91

 

Now my problem is whether we can weld or connect this SA 335 P11 and SA 335 P91 ?

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/f5e2364b-86a7-43d5-91c7-db540299ef3a%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...