Dear Group Members,

Base Material : SA 516 Gr 70  
Thickness   : 60 MM
MDMT   : Minus 45 Deg C

Weld consumables Tested for Impact at Minus 46 Deg C
Code : ASME Section 8 Div 1
Joint : Corner Joints
Weld process : GTAW + SMAW + SAW

Designer says : Weld metal exempt as per UCS-67-a-3

Question :

Requirement of Impact test on WPS  ?
Requirement of Production test coupons ?

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAL9TLdfbnwak067qFAbtfCdfCJ8ZObNLm65iviR3xDpkZ7gCVg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...