Thursday, December 26, 2013

Re: [MW:19725] PQR dia range not qualified and conducted WQT

Mr,Dominic,

As per the Sec IX, diameter is not essential variable. WQT done as per the PQR. Refer QW 256 for GTAW process. I hope you satisfy. 

Pramodh ramanunny
Iraq badra oil feild

Sent from my iPad

On 25-Dec-2013, at 6:26 pm, "Dominic v.k.dominic" <v.k.dominic@gmail.com> wrote:

Dear Experts,

We have qualified PQR test coupon dia 2.5". but WPS not mentioned diameter range qualified
Contractor qualified WQT 1/2" Piping weld,accordingly welding has been done for 3/4" size pipe.  
Please provide your valuable suggestion to these welding accept or reject as per section 1X.

Best Regards,

Dominic V.K.

QA/QC-Inspector.

GAZPROM NEFT BADRA B.V.

Badra Base Camp, Badra, Wasit, IRAQ.

Mobile No +9647823006598.
Think Quality, Safety Tomorrow.
<90902168.gif>

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...