RE: [MW:19706] Using A350/LF2 instead of A105

Please, could yo send us Design Conditions? Pressure and Temperature?

 

 

 

ATENTAMENTE
Antonio Alonso Diaz Arriaga
044 5559952007

De: materials-welding@googlegroups.com [materials-welding@googlegroups.com] en nombre de Ezat Adel [ezatadel2008@gmail.com]
Enviado: sábado, 21 de diciembre de 2013 12:44 a.m.
Para: materials-welding
Asunto: [MW:19666] Using A350/LF2 instead of A105

is there a limitation to use A350/LF2 instead of A105 forged material, there is no low temp. condition the working temp. assumed to be max. 200 C and the impact test is not required.
also as i know A350/LF2 can used from -46C to 345C nd A105 can used from -29C to 427C is this information is documented and if please advice.



--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...