Dear Mr.Bala

Thanks for your quick reply
Can you please explain why we cant perform machining after PWHT and where it was highlighted in the code???

D.Santosh


Date: Mon, 23 Dec 2013 14:26:46 +0530
Subject: Re: [MW:19698] RE:
From: balamuruganqaqc@gmail.com
To: materials-welding@googlegroups.com

No it was not accepted.

Thanks,
Bala


On Mon, Dec 23, 2013 at 2:20 PM, Santosh Dantuluri <santosh-85@hotmail.com> wrote:

From: santosh-85@hotmail.com
To: welding@googlegroups.com
Subject:
Date: Mon, 23 Dec 2013 14:18:44 +0530



Dear experts,

As per API 650(Storage tank) can we proceed for machining on man hole flange face after stress relieving?

Thanks in advance.

Regards
Santossh

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...