Saturday, December 21, 2013

Re: [MW:19669] CS welder can possible SS welding...

 
QW-423 Alternate Base Materials for Welder
Qualification
QW-423.1 Base metal used for welder qualification
may be substituted for the metal specified in the WPS in
accordance with the following table. When a base metal
shown in the left column is used for welder qualification,
the welder is qualified to weld all combinations of base
metals shown in the right column, including unassigned
metals of similar chemical composition to these metals
 
 
 
Qualification Base Metals
P-No. 1 through P-No. 15F, P-No. 1 through P-No. 15F,
P-No. 34, and P-No. 41 P-No. 34, and P-No. 41
through P-No. 49 through P-No. 49
P-No. 21 through P-No. 26 P-No. 21 through P-No. 26
P-No. 51 through P-No. 53 or P-No. 51 through P-No. 53 and
P-No. 61 and P-No. 62 P-No. 61 and P-No. 6


From: tugrulhan özdemir <tugrulhan9@gmail.com>
To: materials-welding@googlegroups.com
Sent: Saturday, 21 December 2013, 9:27
Subject: Re: [MW:19664] CS welder can possible SS welding...

Hi



What about P numbers for CS and SS ?

Saygılarımla / Regards

-
Tuğrulhan ÖZDEMİR
API 653 AI, Welding & Materials Eng.
Iraq mobile number: +964 782 311 67 81



2013/12/8 Brajendra Singh <brajendrasingh523@gmail.com>
yes he is also qualified for ss pipe because as per ASME sec IX addition of inert gas backing is not a essential variable so he is qalifed for both with or without gas purging.


On Sat, Dec 7, 2013 at 10:46 PM, Amit Singh <kshtriya.amit@gmail.com> wrote:
As ASME Sec 9 removal of inert gas backing is essential variable so as per code yes , & same is not for a SS welder welding CS joint
Amit Singh
Sent from my iPhone

On 07-Dec-2013, at 21:25, PK M <pkmqaqc@gmail.com> wrote:

Dear Experts,

Please explain a welder is qualified on ½ inch dia Carbon steel pipe butt joint with GTAW process. So he can weld on ½ inch dia stainless steel pipe butt joint with GTAW process. If any problem for material composition?

Thanks,

Pkm.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to mailto:materials-welding%2Bunsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to mailto:materials-welding%2Bunsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.




Thanks & Regards,
Brajendra  Singh Patel
Welding Engineer
pune, India

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to mailto:materials-welding%2Bunsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to mailto:materials-welding%2Bunsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.


No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...