[MW:19721] PQR dia range not qualified and conducted WQT

Dear Experts,

We have qualified PQR test coupon dia 2.5". but WPS not mentioned diameter range qualified
Contractor qualified WQT 1/2" Piping weld,accordingly welding has been done for 3/4" size pipe.  
Please provide your valuable suggestion to these welding accept or reject as per section 1X.

Best Regards,

Dominic V.K.

QA/QC-Inspector.

GAZPROM NEFT BADRA B.V.

Badra Base Camp, Badra, Wasit, IRAQ.

Mobile No +9647823006598.
Think Quality, Safety Tomorrow.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...