Dear Mervin,
 
If this pipe is related to sour sevice, hardness test is mandatory. Unless you don't have the PQ without hardness requirement, you also need to prepare another PQ to satisfy the requirement.
Hope this help you.

2013년 12월 19일 목요일 오후 12시 35분 55초 UTC+9, mervin dio 님의 말:
dear expert,
 
can any one help me about the hardness test of 1" 316L material as per approved procedure hardness test is required.
 
 
1.my question is in production joint hardness test is needed..we use this in sour service.
 
kid

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...