Friday, February 1, 2013

Re: [MW:16655] SPHERE STORAGE TANK AS PER ASME "U"

Kumar,
Could you définie thé service for such spheres?
If its thé LPG, API 2512 apply 

Sent from my iPad

On Jan 31, 2013, at 5:45 AM, manoj john <manojacgnr@gmail.com> wrote:

Dear experts,

Kindly clear my doubts regarding sphere tank fabrication as per ASME SEC VIII Div  I

1) What is the size of template to check the forming of petals and fitup of petals.
2) Is it mentioned in ASME SECVIII Div 1 the template size for checking sphere tank profile.
3) Can we refer ASME SEC VIII Div 2 for fabrication tolerances since the design is as per div. 1
Thanks & Rgards.
Manoj

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 