Dear sir
This will be deffer Inspection engineer to Inspection Engineer of
EIL, actuvally the 2 no of weld joint on production shall be cover
for each welder, including RT %age of piping class, we did the same
thing in over BPCL Cochin site under EIL inspection and it was
acceptaed
Regards
GSR
On Wed, Feb 20, 2013 at 4:36 PM, LALIT VADADORIYA
<lalit.vadadoriya@gmail.com> wrote:
> Dear Jignesh
>
> As per EIL Spec. for welder qualification after acceptance of WQT test
> piece. It is mandatory to take One No. Production Joint RT( Above 6 Inch
> dia) and 2 Nos. Joints To be requred for 6 Inch and below size for complete
> welder qualification. It is not covered in ndt % of piping class.
>
>
> --
> Regards
>
> Lalit Vadadoriya
> Sr.Engineer (Inspection)
> Engineers India Limited
> Dahej Petrochemical Complex,
> Dahej (Gujarat)
>
> On Tue, Feb 19, 2013 at 1:52 PM, Jignesh Desai <jignesh.desai.met@gmail.com>
> wrote:
>>
>> With ref. to below two paras of the PMC welding specification, Can we
>> consider, these radiographed welds under %NDT (RT) coverage for respective
>> piping class?
>>
>> Where random radiography is specified, the first weld of each welder shall
>> be completely radiographed. In the case of pipe of size 6" and below, the
>> first two welds shall be completely radiographed.
>>
>> For each weld performed by a welder found unacceptable, two additional
>> checks shall be carried out on welds performed by the same welder. This
>> operation is iterative and the of two additional welds for each weld deemed
>> unsatisfactory shall be continued till such time that two consecutive welds
>> of satisfactory quality are found for every defective weld.
>>
>>
>> Regds/Jignesh
>>
>> --
>> To post to this group, send email to materials-welding@googlegroups.com
>> To unsubscribe from this group, send email to
>> materials-welding+unsubscribe@googlegroups.com
>> For more options, visit this group's bolg at
>> http://materials-welding.blogspot.com/
>>
>> http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
>>
>> The views expressed/exchnaged in this group are members personel views and
>> meant for educational purposes only, Users must take their own decisions
>> w.r.t. applicable code/standard/contract documents.
>> ---
>> You received this message because you are subscribed to the Google Groups
>> "Materials & Welding" group.
>> To unsubscribe from this group and stop receiving emails from it, send an
>> email to materials-welding+unsubscribe@googlegroups.com.
>> For more options, visit https://groups.google.com/groups/opt_out.
>>
>>
>
>
>
>
>
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
>
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
> ---
> You received this message because you are subscribed to the Google Groups
> "Materials & Welding" group.
> To unsubscribe from this group and stop receiving emails from it, send an
> email to materials-welding+unsubscribe@googlegroups.com.
> For more options, visit https://groups.google.com/groups/opt_out.
>
>
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
Subscribe to:
Post Comments (Atom)
[MW:35633] IP Joint
Hello experts, I would like to know what is IP joints in piping(31.3)? Regards Saurabh -- https://materials-welding.blogspot.com/...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...
No comments:
Post a Comment