Saturday, February 23, 2013

Re: [MW:16847] Brinell Hardness value for SA 335 P 22 & SA 106 Gr B

Hi!
API spec generaly ask for 235BHN equivalent on HV10 for P22 material
Regards
 
Hegde

--- On Sat, 23/2/13, mohamed jubair <kmd.jubair@gmail.com> wrote:

From: mohamed jubair <kmd.jubair@gmail.com>
Subject: [MW:16845] Brinell Hardness value for SA 335 P 22 & SA 106 Gr B
To: "materials-welding@googlegroups.com" <materials-welding@googlegroups.com>
Date: Saturday, 23 February, 2013, 11:43 AM

Dear all
After PWHT I want to check the hardness of the weldment,heat affected zone,parent metal of the welded joints. What is the brinell hardness value for the below two materials.
Material
SA 335 P22+SA 335 P22
Size
960 X 50 mm
Material
SA 106 Gr A+SA 106 Gr A
Size
540 X 62 mm
Awaiting for reply
Thanks & Regards
Jubair
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...