Re: [MW:16813] WPS for repairing of cast Iron rig material

Preheating, slow cooling and Peening very important. ENiFe CI is ok

On 2/14/13, mahesh deshmukh <deshmukhmd@rediffmail.com> wrote:
> Dear Mr.Ramana
> Please try UTP 81 this products will help you.
>
> On Thu, 14 Feb 2013 13:12:17 +0530 wrote
>>Dear experts
> we faced a problem in repairing of cast iron material for oil rig wheel. We
> used elecrode ENi-Cl but it was failed due to lack of fusion. Can anybody
> suggests if we proceed with ENiFe-Cl elecrode and relared WPS?
>
> --
> Best Regards
> T.V.Ramana
>
>
>
>
> --
>>
> To post to this group, send email to materials-welding@googlegroups.com
>>
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
>>
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
>>
> http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
>>
>
>>
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>>
> ---
>>
> You received this message because you are subscribed to the Google Groups
> "Materials & Welding" group.
>>
> To unsubscribe from this group and stop receiving emails from it, send an
> email to materials-welding+unsubscribe@googlegroups.com.
>>
> For more options, visit https://groups.google.com/groups/opt_out.
>>
>
>>
>
>>
>
>
> Regards
>
> Mahesh Deshmukh
>
> Ph :971504694928
>
> Dubai.
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
>
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
> ---
> You received this message because you are subscribed to the Google Groups
> "Materials & Welding" group.
> To unsubscribe from this group and stop receiving emails from it, send an
> email to materials-welding+unsubscribe@googlegroups.com.
> For more options, visit https://groups.google.com/groups/opt_out.
>
>
>

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...