Yes, Mr Khan is correct. PWHT is not an essential variable.
Thanks,
M. Vedaraju
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Saquib Khan
Sent: Saturday, February 23, 2013 6:30 AM
To: materials-welding@googlegroups.com
Subject: RE: [MW:16843] welder qualified on PWHT wps
Mohd,
Yes they can are qualified. PWHT is not an essential variable per ASME Sec IX for welding performance qualifications.
With Best Regards,
Saquib Khan
> Date: Fri, 22 Feb 2013 20:33:18 -0800
> Subject: [MW:16842] welder qualified on PWHT wps
> From: mohd52100@gmail.com
> To: materials-welding@googlegroups.com
>
> dear all,
> WPS 1 : SMAW +GTAW with PWHT t22,A106 .
> WPS 2 : SMAW +GTAW without PWHT
> t22,A106.
> welders qualified in WPS2 can be utilised to welding wit WPS1.?
> ( PWHT is not essential for welder.).
>
> Regards,
> Mohd.
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at http://materials-welding.blogspot.com/
> http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
>
> The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
> ---
> You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
> To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
> For more options, visit https://groups.google.com/groups/opt_out.
>
>
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
Comments