BS EN ISO 15614 Specification and qualification of welding procedures for metallic materials, Part 13 covers  Resistance butt and flash welding
Also covered in ASME IX , refer QW265
you can refer the following document from Indian Railways.
http://www.indianrailways.gov.in/railwayboard/uploads/codesmanual/MFBWOR/index.htm

On Thursday, February 21, 2013 11:06:48 AM UTC+5:30, AMARAPU SIVAYYA wrote:
Dear Experts 

1.  please give me the code for flash butt weld. where can  get  WPS/ PQR and WPQ formats. 
 
for flash butt weld. 

Material : SAE 1541 
 Size of the material : 75mm X 22mmTh. 
Welding : FLASH BUTT WELD 

2.  I require Geosynthetic material joining welder /seamer qualification record. Please suggest me the available code or  if you have certificate send me a copy. 
--
Thanks with Regards


Sivayya
S2, Brahma Towers
P.No.65, Palace layout.
 Pedawaltair
VISAKHAPATNAM- 530017 (AP)
Mobile : 9346868777

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...