Re: [MW:16818] Effect of High amount of manganese in chemical composition

dear hardik ,
 
the attachment  will give you the clear idea.
 

G.Surya Prakash (C E O), Mobile: +91-9885162668

ASSOCIATED ENGINEERING SERVICES ( An ISO 9001:2008 Certified Company)

Panchavati Mall, Narayanaguda, Hyd-029

Ph.No: (O): +91-40-66830620, E-mail: gajjalla@gmail.com, Website: www.aesinspections.com



 
On Mon, Feb 18, 2013 at 9:52 AM, hardik desai <hvdesai1284@gmail.com> wrote:

can any one tell me the practical relation between carbon and Mn? why increase or decrease in one  will effect the other. is it due to the balance of carbon equivalent or something?
 
Regards,
Hardik...........

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 



--

With Regards,                                                                         

G.Surya Prakash (C E O), Mobile: +91-9885162668

ASSOCIATED ENGINEERING SERVICES ( An ISO 9001:2008 Certified Company) 

Panchavati Mall, Narayanaguda, Hyd-029 

Ph.No: (O): +91-40-66830620E-mail: gajjalla@gmail.com, Website: www.aesinspections.com

 

 

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

No comments:

[MW:35633] IP Joint

Hello experts, I would like to know what is IP joints in piping(31.3)?  Regards Saurabh -- https://materials-welding.blogspot.com/...