[MW:16815] Acceptable Ferritic Range for DSS Needed.

Dear Sir
 Currently we are having the fabrication job of Duplex Stainless Steel.
The Pipes are as per SA 790 UNS 32205 and the flanges are as per SA182 Gr.F51.
The Client has asked us to conduct the ferrite measurement test for the Flanges and Fittings.
Can anybody tell us  what are the acceptable ranges for ferrite content in DSS/SA182/Gr.F 51.?
Please also let me know where in the standard this information can be seen or referred

--
Warm Regards
amit

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...