Thursday, February 21, 2013

Re: [MW:16829] WPS preparation of 48" API 5L x46 pipe.

Dear JD,
               whatever the discussion here is true and useful but in practical, 48" dia. with 2.5 is not feasible to welder in uphill progression and u r having pipe thk 12.7 mm, tell ur client to witness the procedure with 3.2 n check the DT result that can fulfill there requirement and tell them we are quality conscious and responsible for production with quality. its not big issue. as contractor u can propose Pwps, and client only can give u the suggestion they can't force you.    

On Monday, February 18, 2013 6:34:28 PM UTC+5:30, joydev dalai wrote:
Dear BR,
 
U r right our client insist to use 2.5 electrode , but we are poposed for 3.2 mm dia. as per asme dia of electrode is non essential. My question is that if we used 3.2 mm dia electrod, is there any problem? 
On Mon, Feb 18, 2013 at 4:55 PM, Hamed <hamkan...@gmail.com> wrote:

Dear Sir

I think your  client insist to use 2.5 electrode because of complete penetration and fusion not because of the WPS restriction , correct ?

BR

 

From: material...@googlegroups.com [mailto:material...@googlegroups.com] On Behalf Of Binoy Soman
Sent: Sunday, February 17, 2013 10:33 AM
To: material...@googlegroups.com
Subject: RE: [MW:16793] WPS preparation of 48" API 5L x46 pipe.

 

Dear,

 

According to QW-404.6, change in diameter of electrode is a non-essential variable(If there is impact test, change in dia greater than 6 mm is supplementary essential according to 404.7).

If no impact test is required, then you can just revise your WPS as per 200.1 (c ).

 

 

 

Thanks & Regards,

      TEAM QA/QC- SHOAIBA II CCPP

       S.Binoy, Welding Engineer  

     DAELIM Saudi Arabia Co. Ltd.

     Email- bino...@daelim.co.kr

       Mob: 0592633853 / 0508308633

                   

                       "Let Us Believe in TEAM Work (Together   E veryone   Achieves  More)"

 

 

 

From: material...@googlegroups.com [mailto:material...@googlegroups.com] On Behalf Of joydev dalai
Sent: Sunday, February 17, 2013 7:29 AM
To: material...@googlegroups.com
Subject: [MW:16785] WPS preparation of 48" API 5L x46 pipe.

 

Dear all,

 

I have problem for preparation of WPS for 48" API 5L X 46,12.7mm wt. pipe, the WPS criteria meet as per ASME. We are suggest for E6010-3.2 mm dia electrode for Root pass, but our client can't accept for it.

 

They have suggest for E6010 - 2.5mm dia electrode.

 

so please suggest me

 

joydev dalai

Sr. Engg(QA/QC)

Fernas construction india Ltd.

 

--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

No comments:

[MW:35633] IP Joint

Hello experts, I would like to know what is IP joints in piping(31.3)?  Regards Saurabh -- https://materials-welding.blogspot.com/...