Re: [MW:16886] PMI on Stainless Steel Welds

It depends, 
-on which side you are : either client side or manufacturer / contractor side 
-how much you are worried about quality of welds
-situation : of there is only SS work is going on and only one grade and brand of consumable is being used, then it may not required (if specified in client spec then its mandatory)
- Many times manufacturers involved in SS fabrication use lower grade consumables for welding and overlay, hence it is necessary to verify the correct grade (use of 308 instead of 309, 347, 316 welds)
-many other consideration..



On 27 February 2013 08:07, Weaver, mark <Mark.Weaver@honeywell.com> wrote:
Client specified
 
From: Binoy Soman [mailto:binoy.spp@DAELIM.CO.KR]
Sent: Tuesday, February 26, 2013 01:10 PM
To: materials-welding@googlegroups.com <materials-welding@googlegroups.com>
Subject: [MW:16879] PMI on Stainless Steel Welds
 

 

Dear Experts,

 

In a project, Is it always necessary  to do PMI on all Stainless welds or whether it is a clent requirement only. Code followed is ASME B 31.1

 

S.Binoy

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 



--
C. K. Purohit

+968 92840112

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...