Mohd Firdaus Abd Rahim
Dear Experts,
Our company is going to make a new PQR and WPS but since I am new at ASME sec IX and B31.3, I would like to verify my tests before doing them.
So PQR specs are;
Thickness 10mm (WPS qual. 10-15mm)
Mat Plate - SA516 Gr60 & SA516 Gr70 (this will qualify bot P1G1 and P1G2 mats right?)
Preheat 38°C Min(client spec)
Interpass Temp 250°C Max
PWHT 620°C (120min, 100°C/hr)
Pos 3G
Type GTAW + SMAW
Tests:
2 Tensile Test
2 Face Bend Test
2 Root Bend Test
4 Side Bend Test (Do we need this?)
5? Toughness Test (Charpy V-Noch at -46 C is enough?)
Hardness
Radiography
And the other thing is how big test coupon should I weld to get these tests. --
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
Comments