Re: [MW:11215] pittings on surface of Shell

Dear Mr Azmi,
      Please see UG-16 c) Mill Undertolerance for plates of ASME Sec VIII Div. I. 
This allows 0.25 mm less thickness; addition to this please refer Corrosion allowance.
 
Regards,
 
Vikas.

On Fri, May 27, 2011 at 2:14 PM, asad azmi <azmiasadayub@gmail.com> wrote:
Dear All,
 
Greetings.
 
Pittings (not more than 0.5 mm in depth) observed on the surface of a shell of a Vessel. pls find photos for your reference.
 
Shell material  is SA 36. thickness 8mm. service fluid - water
 
Code of construction is ASME SEC VIII DIV1
 
After grindings also pittings can be observed on the large surface of the shell.
 
Whether these pittings can be accepted as it is OR further grinding is required.
 
Please Suggest.
 
Thanks and Regards
 
Asad Azmi

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...