Moisture is problem for defects and it shall be less than 5PPM is always give better result
as u mentioned gas flow rate is too high, pl check again and recommend

On Wed, May 25, 2011 at 6:36 PM, kalyan vvv <vvvkalli@gmail.com> wrote:
Hi mustaffi,
 
It is better to use 99.998% purity of ultra pure argon as a purging & shielding gas.It gives sound quality of welding and better results.
In this other components are
                                         oxygen   -- < 4.00PPM
                                         Moisture -- < 4.00PPM
                                         THC       --  < 0.5PPM
Oxygen & moisture percentage is more than 0.4PPM it may leads to corrosion ,contamination &  porosity.
Maintain gas flow rate between 25 to 40PPM.
 
--
THANKS & REGARDS
 
KALYAN VVV
WELDING ENGINEER
THYSSEN KRUPP INDUSTRIES (INDIA) LTD
HYDERABAD
Mob.NO- 09885273257

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...