Re: [MW:11191] Renewal of Welder Qualification

yes, renewal is for Usage of his welding process( Renewal is only for his qualified welding process0
pandithan

On Sat, May 28, 2011 at 6:29 PM, limesh M <limesh78@gmail.com> wrote:
Dear All,

Welder Qualification Code: ASME BPV SEC IX

I have a qualified welder with following diameter range.

1.1/2'' and above


Now his qualification is going to expire and I would like to renew it by showing supporting radiography reports.

Is it possible to renew the above qualification by showing the radiography report of an 8" diameter pipe?


Regards,

Limesh 


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...