Re: [MW:11182] Renewal of Welder Qualification

Hi,
As per Sec.IX if the welder is not welded with his qualification limits for 6 months of period,his qualification shall be revoked.
But in your case,11/2" dia is also vovers 8".So you can show the RT report as a supporting document for the welder's renewal.

Thanks & Regards,

(Karthik)

Karthikeyan.S
QA/QC Manager
Getabec Energy Co.,Ltd.
379,Moo6,Soi8,Nikhomphatana,
Rayong-21180,
Thailand.
Phone: 0066 38 897035-8 (Off)
Fax: 0066 38 897034
Hand Phone: 0066 892512282


--- On Sat, 5/28/11, limesh M <limesh78@gmail.com> wrote:

From: limesh M <limesh78@gmail.com>
Subject: [MW:11175] Renewal of Welder Qualification
To: "Materials & Welding" <materials-welding@googlegroups.com>
Date: Saturday, May 28, 2011, 7:59 PM

Dear All,

Welder Qualification Code: ASME BPV SEC IX

I have a qualified welder with following diameter range.

1.1/2'' and above


Now his qualification is going to expire and I would like to renew it by showing supporting radiography reports.

Is it possible to renew the above qualification by showing the radiography report of an 8" diameter pipe?


Regards,

Limesh 


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...