RE: [MW:11135] Re : Gas use for Backing and Purging

At TIG shielding and root gases may differ depending on the demands regarding corrosion resistance of the welded joint.

In most cases pure argon will be satisfactory and give a corrosion resistance with enough margin

Regards

 

Di Prinzio, Juan Carlos

 

De: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] En nombre de mustaffi
Enviado el: martes, 24 de mayo de 2011 2:46
Para: materials-welding@googlegroups.com
Asunto: [MW:11130] Re : Gas use for Backing and Purging

 

Hi All

 

Can anybody can tell me, what it’s the best gases to proceed welds for TIG process on Duplex Steel Material

 

Regards

Mus

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

 

__________ Información de ESET Smart Security, versión de la base de firmas de virus 6147 (20110524) __________

 

ESET Smart Security ha comprobado este mensaje.

 

http://www.eset.com



__________ Información de ESET Smart Security, versión de la base de firmas de virus 6147 (20110524) __________

ESET Smart Security ha comprobado este mensaje.

http://www.eset.com

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...