Monday, May 2, 2011

Re: [MW:10912] Hydrotest-API 650

Dhana,

You need to redo the HT if the welding of temporary support attached to pressure part, refer to your tank construction code. Thanks

Regards
RM

Sent by Maxis from my BlackBerry® smartphone


From: SOHAIB GHNAIMAT <sohaib_cegco@yahoo.com>
Sender: materials-welding@googlegroups.com
Date: Sun, 1 May 2011 10:16:21 -0700 (PDT)
To: <materials-welding@googlegroups.com>
ReplyTo: materials-welding@googlegroups.com
Subject: Re: [MW:10909] Hydrotest-API 650

Re-Hydro test should be done.
 
Regards,
 
Sohaib


From: DHANASEKARAN SUBRAMANIAM <subramaniamdhanasekaran7@gmail.com>
To: materials-welding@googlegroups.com
Sent: Sun, May 1, 2011 8:40:39 AM
Subject: [MW:10902] Hydrotest-API 650

Gents,
After the completion of a tank hydro test, some temporary attachment welding has been made on the shell and roof plates.
What action needs to be taken at this stage, kindly provide the action plan with code references.
 
 
Your Immediate response is highly appreciated.
 
 


--
WITH REGARDS,
DHANASEKARAN .S ,
Mob.no: +96893220429.


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...