Who said ...? These electrodes can also root filler and caping, mostly used for welding pipe line or (welding down) ASME XI IS THAT I KNOW

 

RGDS

IBNU

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Viji M
Sent: 29 Mei 2011 12:14
To: materials-welding@googlegroups.com
Subject: [MW:11185] Root Pass Welding

 

Dear Experts,

 

Can you pl share why E 6010 electrode used in Root pass welding ?

 

Best Regards,

Deva

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...