[MW:11184] any one can explain how welding CRACKS looks on x-ray film of any welded pipes ETC. ----

DEAR EXPERTS
                     GOOD DAY
CAN ANY ONE EXPLAIN HOWS CRACKS IN WELD ON X-RAY FILMS LOOKS?
 
IT LOOK LIKE ZIZ ZAG???
ITS LOOKS LIKE THIN/NARROW STRAIGHT LINE???
 
BECAUSE I AM  CONFUSED ABOUT INDICATION OF CRACKS OF WELDING ON X-RAY FILM?
 
 
WAITING FOR REPLY.
 
REGARDS
MOHAMMAD SAZID ALAM
INSPECTION ENGINEER
AICO-DAMMAM
MOBILE:-0534077860

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...