[MW:11162] consumable for s355 JR............


Resp all,
              we established procedure for S355 JR with E7018 in SMAW process. It meets all the mechanical requirements.
              E7018 Electrode is sufficient for welding of S355 JR material  in SMAW process.(Actually this material is european standard material there is no
              exactly equivalent material in  ASTM)
              So It is better to use E7018 electrode.
--
THANKS & REGARDS
 
KALYAN VVV
WELDING ENGINEER
THYSSEN KRUPP INDUSTRIES (INDIA) LTD
HYDERABAD
Mob.NO- 09885273257

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...