Hi mustaffi,
It is better to use 99.998% purity of ultra pure argon as a purging & shielding gas.It gives sound quality of welding and better results.
In this other components are
oxygen -- < 4.00PPM
Moisture -- < 4.00PPM
THC -- < 0.5PPM
Oxygen & moisture percentage is more than 0.4PPM it may leads to corrosion ,contamination & porosity.
Maintain gas flow rate between 25 to 40PPM.
--