Tuesday, May 24, 2011

[MW:11129] RE: 11126] Radiography in U/G Pipelines

Hi,

This will depends on the client specification and design standards, and
respective code.

Frequency of testing (quantity) shall be as per ITP which was agreed between
Client / Contractor

Thanks & Regards

Lakshman kumar.B | Manager - QA/QC | LANCO  INFRATECH LIMITED
Plot# 1255 | Sanjeevani Chowk | Mahanadi Vihar | Cuttack 753004
Phone : + 91-671-2445033| Mobile: +91 9937286851 | www.lancogroup.com
Go Green |The future will thank you: Lakshman.kumar@lancogroup.com,
Lakshmankumar4@gmail.com

-----Original Message-----
From: materials-welding@googlegroups.com
[mailto:materials-welding@googlegroups.com] On Behalf Of Krishnakumar M S
Sent: Monday, May 23, 2011 9:39 PM
To: materials-welding@googlegroups.com
Subject: [MW:11126] Radiography in U/G Pipelines

Hi..

I want to know about the quantity (in %) of Radiography on welded joints for
underground oil pipelines (service: crude oil, naphtha, HSD & MS Regular)
size range: 24" to 40" welded pipes

Any body who know this pls give their valuable comments (any reference
document regarding this, please share to us...)

Regards,

KRISHNAKUMAR
FEDO, Udyogamandal
Cochin, Kerala

----------
Sent from my Nokia phone

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to
materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and
meant for educational purposes only, Users must take their own decisions
w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...