Dear All,
 
Beveling (J-type bevel) before rolling is better and more convenient for process as well as to maintain
the quality.
 

 

Thanks & best regards,

Dharmesh N Patel

Assistant Manager –Package Engineering  

Dresser-Rand India Private Limited.

Naroda, Ahmedabad.

Phone Office + 91-79-228 06415

 

P Please don't print this e-mail unless you really need to.  Save Trees - Save Environment


 


From: Navid Navidi <navid_751400@yahoo.com>
To: material <materials-welding@googlegroups.com>
Sent: Mon, May 2, 2011 12:15:42 PM
Subject: [MW:10920] bevel-plate-rolling

Dear All,

I have a question regarding rolling a plate with 80-100mm thickness.
Which one is better: a) beveling (J-type bevel) before rolling   or
                             b) beveling (J-type bevel) after rolling
 
Is it possible to maintain the quality of the bevel while rolling process?

regards,

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...