Dear Mr.Vishal

The electrodes you are talking about are as per Russian specs.
However in India, they are also made by MIDHANI,hyderabad for defence applications and you cannot purchase these electrodes from local market / consumable manufacturers.

These electrodes are FIM from MIDHANI for defense projects in India !
In past i have used following electrodes in my defence project: EA981/15, EA400/10Y, etc....

Regards

Prem Nautiyal
cell: 9820313278

On Sun, 11 Jul 2010 08:20:53 +0530 wrote
>Thanks John,



Are these only manufactured in Russia? Any other manufacturer you know elsewhere?



Regards



VISHAL MEHTA



SUPERTECH SERVICES LTD



Sent on my BlackBerry® from Vodafone



-----Original Message-----

From: "John Henning"

Sender: materials-welding@googlegroups.com

Date: Fri, 9 Jul 2010 14:30:47

To:

Reply-To: materials-welding@googlegroups.com

Subject: [MW:5922] RE: 5920] EA 395/9



Try the following - Russian electrodes intended for buttering

applications for ferritic to austenitic stainless



http://www.elmics.ru/material/el/el0301_e.htm



http://www.mmk-metiz.ru/eng/content/prices/catalogue/viewdoc_n_en/206



John



-----Original Message-----

From: materials-welding@googlegroups.com

[mailto:materials-welding@googlegroups.com] On Behalf Of Vishal Mehta

Sent: Friday, July 09, 2010 12:42 PM

To: materials-welding@googlegroups.com

Subject: [MW:5920] EA 395/9



Hello,



Can anyone give details of EA 395/9 grade electrode, with its

composition?



Also who are the manufacturers of this electrode and its availability in

India.



Thanks



Regards



VISHAL MEHTA



SUPERTECH SERVICES LTD



Sent on my BlackBerry(r) from Vodafone



--

To post to this group, send email to materials-welding@googlegroups.com

To unsubscribe from this group, send email to

materials-welding-unsubscribe@googlegroups.com

For more options, visit this group's bolg at

http://materials-welding.blogspot.com/

The views expressed/exchnaged in this group are members personel views

and meant for educational purposes only, Users must take their own

decisions w.r.t. applicable code/standard/contract documents.



--

To post to this group, send email to materials-welding@googlegroups.com

To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com

For more options, visit this group's bolg at http://materials-welding.blogspot.com/

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--

To post to this group, send email to materials-welding@googlegroups.com

To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com

For more options, visit this group's bolg at http://materials-welding.blogspot.com/

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



PREM S NAUTIYAL
CELL : 9820313278

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...