No problem with modular fc wehave carried pwht of 25 mt vessel n 250 t. Regards. Hegde
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Sent from my BlackBerry® smartphone from !DEA
From: suresh venkat <atozsuresh@gmail.com>
Sender: materials-welding@googlegroups.com
Date: Fri, 30 Jul 2010 20:48:22 +0900
To: <materials-welding@googlegroups.com>
ReplyTo: materials-welding@googlegroups.com
Subject: [MW:6205] PWHT of Bigger diameter & Long vessels
Dear all,
we have several equipments of diameter 5mts & above & length 30 mtrs & above. Our specs calls for PWHT in an enclosed furnace.
some of our fabricators expressed inability due to furnace size restrictions& informed us that use of Temporary Modular furnaces will pose risk to Quality of final product.
I need your advice on the following
1. Is doing PWHT in modular furnaces will create any problems to the equipment (in terms of quality)
2. can the temperature be properly controlled
3. Pwht can be performed properly without overheating or Under heating.
thanks
Suresh
-- To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments