Dear All,
 
I have one electrode test certificate of E6013 size 2.5 mm of HONAVAR ELECTRODES PVT. LTD.
I have some query on it
1)In sec II part-C SFA 5.1 there is mention that not specified for P,S etc so what is the max.limit of these elements like P,S?
 
2)I have same manufacture other TCs Certified by QA/QC manager but this certificate is not. Can we demand for this?
only signed by preparer.Can we accept this?
 
3)Pl. let me know what is basic requirement for review TC of electrode or filler wire?
 
Thanks,
With Best Regards,
Ramesh Barot