Hi Subrata,

 

Generally, Hastelloy C-276 alloy is  furnished in the solution heat-treated condition unless otherwise specified. C-276 alloy is normally solution heat treated at 2050°F (1121°C) and rapid quenched.

 

Parts which have been hot-formed should be solution annealed prior to final fabrication or installation, if possible.

 

ASME specifications for Hastelloy:-C-276 alloy plate, sheet, strip, bar, tubing and pipe are SB-574, SB-575, SB-619, SB-622 and SB-626 under UNS number N10276. General thumb rule for this alloy is to be supplied in Solution Annealed condition, to ensure highest corrosion resistance and the best mechanical properties.

 

Thanks

 

Pradip Goswami,P.Eng.

Welding & Metallurgical Engineer/Specialist

Email-pgoswami@sympatico.ca,

pgoswami@quickclic.net 

www.opg.com

 

 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of subrata das
Sent: Friday, July 30, 2010 2:28 AM
To: materials-welding@googlegroups.com
Subject: [MW:6199] heat treatment procedure

Dear all

Kindly share your opinion about the heat treatment procedure for SB622 UNS N10276 Nickel Alloy Steel Pipe/Fittings ?  

 

Regards

Subrata Das

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


THIS MESSAGE IS ONLY INTENDED FOR THE USE OF THE INTENDED RECIPIENT(S) AND MAY CONTAIN INFORMATION THAT IS PRIVILEGED, PROPRIETARY AND/OR CONFIDENTIAL. If you are not the intended recipient, you are hereby notified that any review, retransmission, dissemination, distribution, copying, conversion to hard copy or other use of this communication is strictly prohibited. If you are not the intended recipient and have received this message in error, please notify me by return e-mail and delete this message from your system. Ontario Power Generation Inc.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...