[MW:6223] NACE recommendation on Bolts & Nuts Material

Dear All,

Can anybody tell me why NACE Recommends Low Hardness Materials ( ASTM
A193B7M and A194 2HM) for Bots and Nuts Since Bolts & Nuts are not at
all coming in contact with the Corrosive Fluid.

Thanks & Regards

Vineeth Thomas
Piping Engineer

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...