[MW:6203] Weld-o-let welding minimum fillet size requirement

Header pipe thickness is 41mm weldolet thickness 23mm , but other side
of weld-o-let 6mm. Please give me minimum weld metal for header to
weld- o-let joints whether we can weld less than 23mm & if going like
how much minimum fillet length required.

Mohd Mubarish.P.M
Abu Dhabi.
Welding Engineer.