Tuesday, July 27, 2010

[MW:6154] Transverse Crack

I want to know the exact cause off transverse crack observed visually on the surface of the weld.

Welding done with SAW 
Material - SA 516 GR. 70
Thickness- 32 mm
We have done pre heating at temperature 100 deg. C but from top side also check the filler wire material 
after crack are observed which are ok.
Please share your experience with me on this issue.
Regards,
Nilesh

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...