dear yusuf, as per asme sec ix,2tensile,2facebend,2rootbend are
mandatory.u may have macro also.

On 7/29/10, yusufkhan pathan <yusufkhanp97@gmail.com> wrote:
> Dear all,
>
> I have to prepare a PQR with GTAW+SMAW for Super duplex SS Plate of
> UNS 32750 of thickness 8mm.
> Please suggest me the type and references of test to be conducted for
> the specimen as per ASME SecIX.
>
> Thanks in advance.
>
> Regards.
> Yusufkhan
> +91-9916008202
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding-unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>


--
K Harish Kumar, MTech
Consultant for:
Corrosion Metallurgy
Failure Analysis Surface Coating
Thin Films Vacuum Systems QMS.

www.itindt.com

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...