Wednesday, July 28, 2010

[MW:6161] RE: 6154] Transverse Crack

Mostly these crackings are related to hydrogen.

Can you please specify filler metal (wire – flux combination) and hydrogen precautions (redrying?) and thickness.

 

 

With kind regards, mit freundlichem Grüss, salutations, met vriendelijke groet,

 

Ing. Erwin GERING, IWE

 

Corporate Product Manager      - ALW-corp. mktg           - SAW Wire & Flux        

Product Manager                           - ALW-NL & BeLux          - Welding Consumables                                            

(Tel.: 31(0)76 – 54 83 222  ÈMob.: 31(0)6 - 55 87 29 21

Air Liquide Welding_RVB_5.jpg

 

Van: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] Namens waman nilesh
Verzonden: dinsdag 27 juli 2010 18:58
Aan: materials-welding@googlegroups.com; materials-welding@goolegroups.com
Onderwerp: [MW:6154] Transverse Crack

 

I want to know the exact cause off transverse crack observed visually on the surface of the weld.

 

Welding done with SAW 

Material - SA 516 GR. 70

Thickness- 32 mm

We have done pre heating at temperature 100 deg. C but from top side also check the filler wire material 

after crack are observed which are ok.

Please share your experience with me on this issue.

Regards,

Nilesh

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...