[MW:6127] inconell 625 weld cladding on AISI 4130 material
Dear Team members,
It is required to qualify Nickell Alloy 625 overlay (10% FE max) on AISI 4130 at 1/8" minimum finished overlay deposited thickness.
Have anybody ever been faced with this before to share the experiance?
thanks.
Martin.
Hotmail: Trusted email with Microsoft's powerful SPAM protection. Sign up now.
Hotmail: Powerful Free email with security by Microsoft. Get it now.
Subscribe to:
Post Comments (Atom)
[MW:35668] Selection of Filler/Electrode.
Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...
No comments:
Post a Comment