[MW:6195] RE: 6187] Test for PQR of Super Duplex Stainless steel plate UNS32750

In addition to ASME sec IX requirement it is better to qualify as per GS8
specification

Regards

Hegde P.B.

-----Original Message-----
From: materials-welding@googlegroups.com
[mailto:materials-welding@googlegroups.com] On Behalf Of yusufkhan pathan
Sent: Thursday, July 29, 2010 3:32 PM
To: Materials & Welding
Subject: [MW:6187] Test for PQR of Super Duplex Stainless steel plate
UNS32750

Dear all,

I have to prepare a PQR with GTAW+SMAW for Super duplex SS Plate of
UNS 32750 of thickness 8mm.
Please suggest me the type and references of test to be conducted for
the specimen as per ASME SecIX.

Thanks in advance.

Regards.
Yusufkhan
+91-9916008202

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to
materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and
meant for educational purposes only, Users must take their own decisions
w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...