I too agree; SAW filler wire may not be tested for Mech properties as
the properties are purely based on the flux combination. if the client
is very particular about the mech properites, an all weld test piece
can be tested at lab for mech properties as per spec.

Thanks

On Jul 26, 11:07 pm, "krishna " <w...@rediffmail.com> wrote:
> Frnds,
>        Here i received one SAW Wire test certificate for ESAB OK AUTOROD 12.22L ,as per ASME SEC II Part c SFA 5.17 EM12K.
>
> In the Test certificate they gave only Chemical Analysis of the wire .
>
> Shall I accept the Test certificate or I have to ask for Mechanical Properties also.
>
> Is it acceptable the Test certficate as it is.    
>
> Kindly guide,
>
> thanks,
> KK

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...