Hi,
for CE upto 0.46 & WT  upto 12.7 mm , you can use 10deg celsius as preheat temp.

On Sun, Jul 18, 2010 at 6:29 PM, shibu simon <shibusimon2000@yahoo.co.uk> wrote:
Hi priama
 
PQR test coupon thickness is 12.7 mm. and CE - 0.38
Regards.
 
shibu

--- On Sun, 18/7/10, pirama rayan <piramarayan@gmail.com> wrote:

From: pirama rayan <piramarayan@gmail.com>
Subject: Re: [MW:6011] Pre heat temperature
To: materials-welding@googlegroups.com
Date: Sunday, 18 July, 2010, 10:53


Dear Shibu
 
What is thickness range of the pipe and CE value ?
 
Piramarayan B

On Sat, Jul 17, 2010 at 9:08 PM, shibu simon <shibusimon2000@yahoo.co.uk> wrote:
Dear all,

Carbon steel base metal initial temperature was 32 deg celcius, during PQR qualification as per API 1104. Decreasing pre heat temperature is an essential variable as per API 1104. So what minimum preheat temperature to give in WPS.

Thanks.

shibu simon




--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
Regards
AAKARSH PP
QA/QC-Welding
LTCS Shop-Hyundai Engg. & Construction
Karan Gas Field Development Project

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35738] ASME IX WPS Qualification Query: GTAW + FCAW with Multiple PQRs

Dear Welding Experts, I'm currently preparing a Welding Procedure Specification (WPS) and have encountered a request to qualify a GTAW +...