Re: [MW:5930] PQR (QW-204b)

Dear All,
 
Reply given by Mr. Jignesh Makwana is quite wrong.
 
As per QW-451.1 Deposited weld metal thk qualification range should be 2t only.
 
wherer as t = Deposited weld metal thk.
 
Regards,
Bhavesh Patel

On Sat, Jul 10, 2010 at 9:39 AM, manpreet <manpreetsin88@rediffmail.com> wrote:
Hi


Accoding to QW 200.4:-
A combination of processes can be used for PQR, if THK of test coupon is at least 13 mm.

Since thk mentioned is more than 13mm So it is qualified for Multiprocess welding.

Max. deposited thickness qualified for each process shall be 2*t.

So your ranges are qualified & can be recorded in WPS.


Regards
Manpreet Singh
Ass. Welding Engineer
Spiecapag
















Hi,



Have the following question regarding weld metal deposition
on PQR with combined GTAW & MMAW processes.

Have recorded both GTAW = 3.5mm & MMAW = 9.8mm onto PQR
(QW-204b) but unsure of the ranges qualified

for both and should they be recorded on associated WPS.



Thanks

QA/QC













--
>
To post to this group, send email to materials-welding@googlegroups.com
>
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
>
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
>
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
>

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...