Re: [MW:5914] Uphill Vs Downhill Welding

Only the welder's qualification is affected by the change of progression

Dr. G. Dilintas - Authorized Inspector Supervisor
I&F Regional Technical Manager
Bureau Veritas Piraeus - Greece
Tel: +30 210 40 63 113/4
Fax: +30 210 40 63 118
Cell: +30 69 44 64 62 04
Inactive hide details for HarikrishnanS@punjlloyd.comHarikrishnanS@punjlloyd.com


          HarikrishnanS@punjlloyd.com
          Sent by: materials-welding@googlegroups.com

          08/07/2010 08:21

          Please respond to
          materials-welding@googlegroups.com

To

materials-welding@googlegroups.com

cc


Subject

[MW:0] Uphill Vs Downhill Welding

Ref



Dear Friends

What is the criteria for selecting Uphill/Downhill weld progression in a Pipeline/Piping? Is it mandatory to use uphill progression in a WPS qualified under ASME Sec IX ?

Thanks and Regards

Harikrishnan N S
Punj Lloyd Ltd, Mumbai


They can, because they think they can.......



---------------------------------------------------------------------------------------------------------------------------------------------------------------------------------------------------------------------


This e-mail and any files transmitted with it are for the sole use of the intended recipient(s) and may contain confidential and privileged information. If you are not the intended recipient of this communication, we request you to notify the sender immediately by return email and destroy all copies and the original message. Any unauthorized review, use, disclosure, dissemination, forwarding, printing or copying of this email is strictly prohibited. The recipient acknowledges that Punj Lloyd Limited or its subsidiaries and associated companies (collectively "Punj Lloyd Group") are unable to exercise control or ensure or guarantee the integrity of/over the contents of the information contained in e-mail transmissions and further acknowledges that any view, opinion or advice expressed in this message are those of the individual sender and no binding nature of the message shall be implied or assumed unless the sender does so expressly with due authority of Punj Lloyd Group. Although we have taken all reasonable precautions to ensure that this communication is free from viruses. We do not assume responsibility for any loss or damage arising from the use of this email.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...