Stephen,
 
The following is the range qualified for the weld metals.
 
GTAW - 7.0 mm max
MMAW - 19.0 mm max
 
Ankur.

On Fri, Jul 9, 2010 at 5:06 AM, Stephen Milne <sim@aalborg-industries.com.au> wrote:

Hi,

 

Have the following question regarding weld metal deposition on PQR with combined GTAW & MMAW processes.

Have recorded both GTAW = 3.5mm & MMAW = 9.8mm onto PQR (QW-204b) but unsure of the ranges qualified

for both and should they be recorded on associated WPS.

 

Thanks

QA/QC

 

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...