Welding uphill, or welding from the bottom to the top on vertical welds, provides much more penetration than welding downhill. Therefore, it is required in most instances to weld uphill by the industry.

In down hill welding the penetration and thickness of weld metal deposited in each layer is very less compared to uphill and completion time of joint is less than down hill. Generally down hill used in UG cross country pipe line as per API1104 other than all only used uphill welding including the compressor station, SV station also.

 

Mostly the client spec/code requirement in pressure vessel and process piping, AG piping used only up hill welding and also the filler or electrode manufacturer specification with respect to ASME sec II C

 

Note: Dear Bhavesh – I have special exp. With your comp. in single joint half portion up hill and another half down hill and make argument like "what will happen?" Don't generalize or deviate the good engineering practice in welding industry as per WPS is welding progression as Non essential (405.3)  but the application wise different.
 
Regards,
PSR.
 


On Thu, Jul 8, 2010 at 12:22 PM, Bhavesh Patel <bhaveshpatel.me@gmail.com> wrote:
Dear Harikrisnan,
 
It is not mandatory to do the welding in Uphill progression as per ASME Sec. IX.
 
See Clause No. QW-405.3 for better explanation.
 
If you change a progression in vertical welds then please check, is the welding consumable is recommended to weld in the same progression?
 
Check with respect to ASME Sec.II Part C.
 
 
Regards,
BHAVESH PATEL
Welding Engg.
ISGEC, DAHEJ
GUJARAT, INDIA

On Thu, Jul 8, 2010 at 10:51 AM, <HarikrishnanS@punjlloyd.com> wrote:

Dear Friends

What is the criteria for selecting Uphill/Downhill weld progression in a Pipeline/Piping? Is it mandatory to use uphill progression in a WPS qualified under ASME Sec IX ?

Thanks and Regards

Harikrishnan N S
Punj Lloyd Ltd, Mumbai


They can, because they think they can.......


---------------------------------------------------------------------------------------------------------------------------------------------------------------------------------------------------------------------


This e-mail and any files transmitted with it are for the sole use of the intended recipient(s) and may contain confidential and privileged information. If you are not the intended recipient of this communication, we request you to notify the sender immediately by return email and destroy all copies and the original message. Any unauthorized review, use, disclosure, dissemination, forwarding, printing or copying of this email is strictly prohibited. The recipient acknowledges that Punj Lloyd Limited or its subsidiaries and associated companies (collectively "Punj Lloyd Group") are unable to exercise control or ensure or guarantee the integrity of/over the contents of the information contained in e-mail transmissions and further acknowledges that any view, opinion or advice expressed in this message are those of the individual sender and no binding nature of the message shall be implied or assumed unless the sender does so expressly with due authority of Punj Lloyd Group. Although we have taken all reasonable precautions to ensure that this communication is free from viruses. We do not assume responsibility for any loss or damage arising from the use of this email.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
Regards

Sethu Ramalingam.p

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...