Re: [MW:5896] 6GR qualified welder. As per AWS D1.1

Philip,
Please give more details on the PQR and production weld.
Shank
08037756442

--- On Fri, 2/7/10, Philip, Taiye (Lagos) <Taiye.Philip@deltaafrik.com> wrote:

From: Philip, Taiye (Lagos) <Taiye.Philip@deltaafrik.com>
Subject: [MW:5828] 6GR qualified welder. As per AWS D1.1
To: materials-welding@googlegroups.com
Date: Friday, 2 July, 2010, 6:29 PM

Hello gents,

 

 I have a query on butt joint welding with 6GR qualified welder. As per AWS D1.1 (2006) Table 4.10 Note d, 6GR qualified welder is qualified for all position. However, they are not qualified to weld production weld butt joint welded from one side without backing or welded from both side without backing. In this case, it is considered as single side welding without backing. Pls could some one in the house clarify more on these if I am right or wrong as per D1.1 interpretations?

 

 

Regards

Philip Taiye

Principal QA/QC Welding Engineer

(MIPs Quality Control)

DeltaAfrik Engineering Limited

2nd Floor, City Express Bank Building

Plot 1637 Adetokunbo Ademola Street

Victoria Island, Lagos   Nigeria

Phone: +234-1-461-8508, +2341-461-6137 ext. 1257
Cell: +234-(0)-803-803-1396
Fax: +234-1-262-2418

e-mail: taiye.philip@worleyparsons.com

 

 


*** WORLEYPARSONS GROUP NOTICE *** "This email is confidential. If you are not the intended recipient, you must not disclose or use the information contained in it. If you have received this email in error, please notify us immediately by return email and delete the email and any attachments. Any personal views or opinions expressed by the writer may not necessarily reflect the views or opinions of any company in the WorleyParsons Group of Companies."

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...