Re: [MW:5888] VESSEL Reinforcement pad Installation

Dear Pravin,
 
As you clarify in your earlier mail that PWHT is not required for vessel (Pressure Part) then there is no need of any PWHT for pad welding though its a non pressure part.
 
Regards,
Bhavesh Patel
Welding Engg.
ISGEC, Dahej,
Gujarat, INDIA

On Wed, Jul 7, 2010 at 1:02 PM, Praveen Kumar <praveenkumar.sek@gmail.com> wrote:
Dear Mr.Karthik,
 
Thanks for your explanation.
 
This is a saddle pad and it's POST WELD HEAT TREATMENT is  required or not for this vessel as per Std.
 
Pad MOC - SA 516 Gr.60 (10 mm thkX150 wideX555 long)
 
pls.advise me the above "PWHT" aspects.
 
 
Thanks & Regards,
 
Praveen Kumar

 

 


On Wed, Jul 7, 2010 at 7:59 AM, Karthik <karthik6684@yahoo.com> wrote:

Hi,

The Contractor is right,Normally Pneumatic test will be done of Re-Inforcement Pad of Nozzles only.In your case this is just a pad plate to avoid shell material directly welded to another kind of material.No need to do Pneumatic test on this.


Thanks & Regards,


(karthik)


Karthikeyan.S
 
Getabec Energy Co.,Ltd.
379,Moo6,Soi8,Nikhomphatana,
Rayong-21180,
Thailand.
Phone: 0066 38 897035-8 (Off)
Fax: 0066 38 897034
Hand Phone: 0066 892512282


--- On Tue, 7/6/10, Praveen Kumar <praveenkumar.sek@gmail.com> wrote:

From: Praveen Kumar <praveenkumar.sek@gmail.com>
Subject: [MW:5877] VESSEL Reinforcement pad Installation
To: materials-welding@googlegroups.com
Date: Tuesday, July 6, 2010, 8:21 PM

Dear members,

Gas Discharge Volume Bottle (508 O.DX2083 LG) Reinforcement pad -2 nos are missing which is used for sitting the vessel on the roller support

This pad is located in between Vessel & roller Support.

Fluid service: Gas

 The Pad Re-Installation will be rectified at site.

Contractor says that there is NO POST WELD HEAT TREATMENT for this vessel also this is a saddle pad and doesn't require pneumatic test of pad which is acceptable or not.

Pls. clarify this issue.
 
 
Thanks & Regards,
Praveen Kumar




--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
Regards,

Praveen Kumar
Mechanical Engineer

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...